Quantachrome Nova 2000E

Summary of Technique
- The NOVA e-Series of surface area analyzers offers a full line of rapid, high throughput B.E.T. surface area and pore size analyzers.
- It uses a nitrogen absorption/desorption process to characterize powders and pellets.
- Analyzes up to 200 data points (100 adsorption points and 100 desorption points).
- Two samples are dried and analyzed simultaneously- at different temperatures if required
Information Provided and Detection Limits
Information Provided
- single and multi-point BET surface area measurements
- pore size distribution
- total pore volume
- average pore radius
Detection Limits
- Measurement types: B.E.T., STSA, adsorption isotherm, desorption isotherm.
- Surface area range: 0.01 m2/g to no known upper limit.
- Pore size range: 0.35 to >500nm (3.5 to >5000 Å)
- Minimum pore volume: (liquid) 2.2 x 10-6 ml/g
- Minimum pore volume: (STP) 0.0001 cc/g
- Temperature Range: ambient - 450 ºC*, 1º C intervals
- Temperature Range: ambient - 450 ºC*, 1º C intervals
Point of Contact
Point of Contact: Dennis Ndaya
dennis.ndaya@uconn.edu
860-486-2568
Industrial Affiliates are encouraged to contact
Co-Director, Hatice Bodugoz-Senturk
Hatice.Bodugoz_Senturk@uconn.edu
860-486-1040